DRK-B1 Industrial Computer Differential Scanning Calorimeter

Short Description:

Rubber thickness gauge is suitable for measuring the thickness and uniformity of vulcanized rubber and plastic products. The thickness gauge complies with the relevant provisions of GB527 "General Requirements for Physical Testing Methods of Vulcanized Rubber"


Product Detail

Product Tags

DRK-B1 Industrial Computerized Differential Scanning Calorimeter supports the testing of multiple parameters such as oxidation induction period, melting point, cold crystallization, solidification, glass transition temperature, specific heat capacity, etc., customer one-key operation, and the software runs fully automatically.

Technical Features:
1: Support the testing of multiple parameters such as oxidation induction period, melting point, cold crystallization, solidification, glass transition temperature, specific heat capacity, etc., customer one-key operation, and the software runs fully automatically.
2: Brand new sensor sample holder, fully enclosed structure design, to prevent items from falling into the furnace body.
3: The instrument meets the following national standards, but not limited to the following national standards:
GB/T 19466.2–2004/ISO 11357-2: 1999 Part 2: Determination of glass transition temperature;
GB/T 19466.3–2004/ISO 11357-3: 1999 Part 3: Determination of melting and crystallization temperature and enthalpy;
GB/T 19466.4–2016/ISO 11357-4: 1999 Part 4: Determination of specific heat capacity;
GB/T 19466.6-2009/ISO 11357-3: 1999 Part 6: Oxidation induction period Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT).
4: Built-in 10-inch super industrial-grade computer, no need for additional computer, integrated equipment, rich display information, including set temperature, sample temperature, oxygen flow, nitrogen flow, differential heat signal, various switch status, flow return zero.
5: The right side of the instrument is equipped with four USB ports as standard, which is convenient for users to connect external devices such as mouse, keyboard, printer, U disk, etc., which is convenient for users to use.
6: The internal USB communication interface of the instrument, compared with the original instrument, has stronger stability, strong versatility, reliable and uninterrupted communication, and supports self-recovery connection function.
7: The digital gas mass flow meter automatically switches the two-channel atmosphere flow, with fast switching speed and short stabilization time.
8: Standard samples are standard, which is convenient for customers to calibrate the constant temperature coefficient.
9: Pre-installed software, no computer adaptability problems, reducing connection problems caused by changing computers and installing driver errors.
10: Support user self-programming program to realize full automation of measurement steps. The software provides dozens of instructions, and users can flexibly combine and save the instructions according to their own measurement steps. Complex operations are simplified into one-key operations.
Applications:
1: Differential scanning calorimeter, which measures the relationship between temperature and heat flow related to the internal thermal transformation of the material, and has a wide range of applications, especially the research and development, performance testing and quality control of materials. The characteristics of materials, such as glass transition temperature, cold crystallization, phase transition, melting, crystallization, product stability, solidification/crosslinking, oxidation induction period, etc., are the research areas of differential scanning calorimeters.
2: Differential scanning calorimeter application range: polymer material solidification reaction temperature and thermal effect, material phase transition temperature and thermal effect measurement, polymer material crystallization, melting temperature and thermal effect measurement, polymer material glass Transition temperature.

Technical Parameter:
1: Temperature range: room temperature~500℃
2: Temperature resolution: 0.01℃
3: Heating rate: 0.1~80℃/min
4: Temperature control method: heating, constant temperature (automatic program control)
5: DSC range: 0~±500mW
6: DSC resolution: 0.001mW
7: DSC sensitivity: 0.001mW
8: Power supply: AC 220V 50Hz or customized
9: Atmosphere control gas: nitrogen and oxygen (the instrument automatically switches)
10: Gas flow rate: 0-200mL/min
11: Gas pressure: 0.2MPa
12: Gas flow accuracy: 0.2mL/min
13: Optional crucible: aluminum crucible Φ6.7*3mm
14: Parameter standard: equipped with standard materials (indium, tin, zinc), users can calibrate the temperature and enthalpy by themselves
15: Data interface: standard USB interface (built-in interface, no need for external connection)
16: Display mode: 10-inch industrial computer touch display, can be connected with mouse, keyboard, U disk, printer

Configuring Single:
1. Differential scanning calorimeter DRK-B1 1 set
2. Built-in industrial computer 1
3. 500 aluminum crucibles
4. 50 ceramic crucibles
5. One standard test sample (indium, tin, zinc, silver)
6. 1 power cord
7.USB cable 1
8. Instruction 1 copy
9. 1 copy of certificate
10. 1 copy of quality guarantee
11. 1 pair of tweezers
12. 1 medicine spoon
13. Oxygen and nitrogen pipes 5 meters
14. Softdog 1
15. Customized pressure reducing valve connector 2 pcs
16.Quick coupler 2
17. 1 software CD
18.Fuse glass fuses 4 pcs
19. Mouse and mouse pad 1 set
20. Keyboard 1


  • Previous:
  • Next:

  • Write your message here and send it to us

    Products categories